COX 764 MITSUBISHI 3 Layer BOPP Coextrusion Line With KATAOKA SLKA 700 Primary Slitter
Year 1989
Capacity: 600 MT/month
Maximum Speed: 220 mpm
Film Width (with edge): 5800 mm
Description
Year 1989
Capacity: 600 MT/month
Maximum Speed: 220 mpm
Film Width (with edge): 5800 mm
- Feeding Hopper : Type SV mixer, Cap 1 m3
- Main Extruder 1 : Ø Screw 135, Speed 38-490 Rpm, L/D Ratio 17, Include Feed Throat Portion
- Main Extruder 2 : : Ø Screw 175, Speed 10-130 Rpm, L/D Ratio 20, Include Melt Feed Portion
- Satelite Extruder A and B
- Ø Screw 75mm Barrier Type, Speed 10.5-105 Rpm, L/D Ratio 29, Include Feed Throat Portion
- Output Max 70 Kg/Hours
- Die : 3 Layer Die, Type Three Cavity T-Die With Flexible Lips
- Width Lips 800m Gap of Lip 2.4 +- 0.7mm Adjust by Push Pull
- Bolt Adjusting Bolt with APC Unit
- Casting Machine : Speed 5-50m/min, Sheet thickness 0.5-3.0mm
- Temperature Range 20-80 Celcius Degree
- Cooling Roll Diameter 1000 (1 Pcs) 1200 (2 Pcs) Surface 0.2 Micron (Mirror)
- Thickness Gauge (Between Cast – MD Section), and PRS Section for Film Scanner Completed Set
Install New one with Thermofisher at 2015
- Longitudinal Strecthing Machine (MDO)
- Speed
- Low Speed Section 5-50 m/min
- High Speed Section 22-220 m/min
- Temperature: Low Speed Section 100-150 Celcius Degree, High Speed Section 70-150 Celcius Degree
- Tenter Frame Machine (TDO)
- Machine Speed 22-220 m/min
- Working Width Inlet 500-800mm
- Outlet 5000-5800 mm
- Film Thickness Inlet120-500 Micron,
- Outlet 12-50 Micron
- Stretching Ratio Max 1:10
- Pull Roll Stand Machine
Consist of
- Trimmer Section : Machine Speed 22-220 m/min
- Treater Section : Machine Speed 22-220 m/min
Winder
- Machine Speed 22-220 m/min
- Max Winding Diameter Ø 800
- Core Steel Ø400 x 5800 mm